218WJ nau'in butene ne mai layi mai ƙarancin yawa wanda ba shi da polyethylene TNPP wanda ya dace da marufi na yau da kullun. Yana da sauƙin sarrafawa wanda ke ba da kyawawan halaye na tauri, ƙarfin tasiri da kaddarorin gani. 218WJ ya ƙunshi ƙarin abubuwa masu zamewa da hana toshewa.
Kadarorin
Fim ɗin lamination, siraran layuka, jakunkunan siyayya, jakunkunan ɗaukar kaya, jakunkunan shara, fina-finan da aka haɗa, marufi na mabukaci da sauran aikace-aikacen gabaɗaya.
DUKIYOYI
DABI'U MASU AL'ADA
RAKUNAN
HANYAR GWAJI
GIDAN POLYMER
Yawan Gudun Narkewa
a 190°C da kuma 2.16 kg
2
g/minti 10
ASTM D1238
Yawan yawa
918
kg/m³
ASTM D1505
KIRA
Maganin zamewa
√
-
Hanyar SABIC
Wakilin hana toshewa
√
-
Hanyar SABIC
GIDAN GANIN GANI
Hazo
13
%
ASTM D1003
Mai sheƙi
a 60°
80
-
ASTM D2457
DUKIYOYIN FIM
Halayen Tashin Hankali
damuwa a lokacin hutu, MD
35
MPa
ASTM D882
damuwa a lokacin hutu, TD
29
MPa
ASTM D882
wahala a lokacin hutu, MD
700
%
ASTM D882
wahala a lokacin hutu, TD
750
%
ASTM D882
damuwa a yawan amfanin ƙasa, MD
12
MPa
ASTM D882
damuwa a yawan amfanin ƙasa, TD
10
MPa
ASTM D882
1% secant modulus, MD
220
MPa
ASTM D882
1% secant modulus, TD
260
MPa
ASTM D882
Juriyar huda
63
J/m
Hanyar SABIC
Ƙarfin Tasirin Dart
85
g
ASTM D1709
Ƙarfin Hawa na Elmendorf
MD
130
g
ASTM D1922
TD
320
g
ASTM D1922
DUKAN thermal
Wurin Tausasawa na Vicat
98
°C
ASTM D1525
(1) An auna halayen injina ta hanyar samar da fim ɗin 30 μ tare da BUR mai ƙarfin 100%218NJ.
Yanayin Sarrafawa
Yanayin sarrafawa na yau da kullun don 218WJ sune: Zafin narkewa: 185 - 205°C, rabon busawa: 2.0 - 3.0。
Dokokin Hulɗa da Lafiya, Tsaro da Abinci
Resin 218WJ ya dace da aikace-aikacen tuntuɓar Abinci. An bayar da cikakkun bayanai a cikin Takardar Bayanan Tsaron Kayan da suka dace kuma don ƙarin takamaiman bayani tuntuɓi wakilin yankin SABIC don samun takardar shaida. SANARWA: Ba a yi nufin wannan samfurin ba kuma bai kamata a yi amfani da shi a cikin kowane aikace-aikacen magunguna/likita ba.
Ajiya da Sarrafawa
Ya kamata a adana resin polyethylene ta yadda zai hana fuskantar hasken rana kai tsaye da/ko zafi. Ya kamata kuma wurin ajiyar ya kasance bushe kuma zai fi kyau kada ya wuce 50°C. SABIC ba zai ba da garanti ga mummunan yanayin ajiya ba wanda zai iya haifar da lalacewar inganci kamar canjin launi, wari mara kyau da rashin aikin samfurin. Yana da kyau a sarrafa resin PE cikin watanni 6 bayan isarwa.