Ya kamata a adana resin polyethylene ta yadda zai hana fuskantar hasken rana kai tsaye da/ko zafi. Ya kamata kuma wurin ajiyar ya kasance bushe kuma zai fi kyau kada ya wuce 50°C. SABIC ba zai ba da garanti ga mummunan yanayin ajiya ba wanda zai iya haifar da lalacewar inganci kamar canjin launi, wari mara kyau da rashin aikin samfurin. Yana da kyau a sarrafa resin PE cikin watanni 6 bayan isarwa.